Leaching of uranium ores in the process of sodium sulphate electrolysis
When uranium is extracted from concentrates with high silicon content, acid leaching is usually used. The disadvantage of this method is the high consumption, high cost and corrosion activity of the reagents. Moreover, for the oxidation of tetravalent uranium to highly soluble hexavalent uranium, it...
Gespeichert in:
Datum: | 2019 |
---|---|
Hauptverfasser: | , , |
Format: | Artikel |
Sprache: | English |
Veröffentlicht: |
Національний науковий центр «Харківський фізико-технічний інститут» НАН України
2019
|
Schriftenreihe: | Вопросы атомной науки и техники |
Schlagworte: | |
Online Zugang: | http://dspace.nbuv.gov.ua/handle/123456789/195228 |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Назва журналу: | Digital Library of Periodicals of National Academy of Sciences of Ukraine |
Zitieren: | Leaching of uranium ores in the process of sodium sulphate electrolysis / V.G. Nefedov, Yu.E. Sknar, O.A. Kharytonova // Problems of atomic science and technology. — 2019. — № 5. — С. 113-117. — Бібліогр.: 2 назв. — англ. |
Institution
Digital Library of Periodicals of National Academy of Sciences of UkraineZusammenfassung: | When uranium is extracted from concentrates with high silicon content, acid leaching is usually used. The disadvantage of this method is the high consumption, high cost and corrosion activity of the reagents. Moreover, for the oxidation of tetravalent uranium to highly soluble hexavalent uranium, it is necessary to process it with oxidizing agents, for example, oxygen. The work shows the possibility of development and chemical concentration of uranium ores using electrolysis of sodium sulfate. During electrolysis the pH in the anode chambers ranges from 2.2…2.5 to 0.5…0.7 in the near-electrode layer of the electrolyte, which corresponds to the pH range during leaching in agitators. Oxygen released at the anode is able to oxidize uranium to hexavalent one. |
---|