Compressive creep of Fe3Al-type iron aluminide with Zr additions
High-temperature creep ofa Fe3Al-type iron aluminide alloyed by zirconium was studied in the temperature range 873-1073 K. The alloy contained (wt.%) 31.5% Al, 3.5% Cr, 0.25% Zr, 0.19% C (Fe balance). It was tested in two states: (i) as received after hot rolling and (ii) heat treated (1423 K/ 2 h/a...