Вплив водню, орієнтації гідридів та температури на опір малоциклової втоми оболонок твелів зі сплаву Zr-1%Nb
Low-cycle fatigue testing was conducted on annular samples with an outer diameter of 9.13 mm, a wall thickness of 0.68 mm and a width of 2.7 mm, namely: non-hydrogenated samples (cut out of standard Zr‑1%Nb cladding tubes); hydrogenated samples with a hydrogen concentration of 50 ... 400 ppm; sample...